8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao

Short Description:


Product Detail

Product Category

Product Tags

Related Video

Feedback (2)

Our merchandise are commonly identified and dependable by end users and will meet continually altering financial and social desires for 7018 Dc Welding Rod , Ss 304 Welding Rod , 2.5 Welding Rods , Customers' reward and fulfillment are usually our biggest objective. Please make contact with us. Give us a probability, provide you with a surprise.
8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao Detail:

Applications:

E6013 welding powder for making welding electrode, which is a kind of carbon steel electrode with iron powder titania type coating. AC/DC. All-position welding. It has excellent welding performance and is almost spatter-free. It has easy re-ignition, good slag detachability, smooth welding appearance. Common grade and rutile grade for you to choose.

Features:

1.Quick strike & Easy restrike & Easy slag-removal
2.Stable arc performance & minimal arc interference
3.Smooth and shiny appearance & Excellent mechanical properties
4. High efficiency and high impact values at -30c.
5. High deposition rates
6. Excellent crack resistance and x-ray performance
7. Packing: 300kgs damproof bag packaging; or as you required

Attention:

1.Electrode must be approved by 350-380℃ for 1 hour before welding, dry the electrode when use it.
2. The rust, oil, water and other impurities of the weld must be removed before welding.
3.You must use short arc welding,the swings should not be too large, narrow bead welding is appropriate.
4. To prevent producing arc porosity, arc plate should be adopted or use return method for arc welding.

Chemical Composition:

Elements TiO2 AL2O3 SiO2 Mn CaO+MgO Organic Other
Actual result 42 4.5 28 9 10.5 4 2

Welding electorde powder of E7018, E6011, E6010, E7024, etc are also available. Pls contact us for more details.

Process technical requirements:

Important welding parts should be clearly marked in accordance with relevant regulations when preparing welding procedure specifications.

Assembling the mold (assembly fixture) of the welded parts, the amount of welding shrinkage must be considered. It should be ensured that the tolerances of the welded parts are within the design requirements.

Before assembling, remove the rust, oil, dust and moisture within no less than 25mm on both sides of the weld. For important welds of low-alloy structural steel, oxide scale should be removed.

The assembly gap should be controlled during assembly. The gap of butt welds is 2~3mm, and the gap of fillet welds is 0~2mm. When the local gap is too large, try to trim it to the specified size. It is strictly forbidden to add fillers in the gap, and strong pairing is prohibited to reduce the residual stress in the welded components.

The welding materials and process parameters used in the assembly tack welding shall be the same as the formal weld requirements.

Welding operations can only be carried out after the welding parts have passed the assembly inspection.

For new materials and new processes, process tests must be done and they can be used only after they are qualified.

The welding slag and defects at the root of the weld must be removed before welding the reverse weld of the weld and other grooved welds

Welding can only be performed after cleaning.

Before welding, it is forbidden to start arc ignition and test current adjustment in the non-welding area. After welding, the surface of the weld should be cleaned and dried.

Net, for important welding parts of important welding parts, the welder’s mark should be marked in the appropriate position after welding.

For steel plates with a thickness of 0.3~4mm, welding methods such as gas metal arc welding or argon tungsten arc welding are mainly used.

For the welding of dissimilar steel components, electrodes, wires and fluxes of the same strength grade should be selected.

When welding low-alloy structural steel, it is not advisable to stop in the middle, and try to complete the welding at one time; during multi-layer welding, the joints between layers should be staggered and the temperature between layers should be controlled between 250~300℃. Before welding the next layer of welding seam, it should be cleaned. Check the weld of the upper layer to ensure that there are no defects.


Product detail pictures:

8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao detail pictures

8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao detail pictures

8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao detail pictures

8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao detail pictures


Related Product Guide:
The composition of the welding electrode

Dependable high-quality and fantastic credit standing are our principles, which will help us at a top-ranking position. Adhering to your tenet of quality very first, client supreme for 8 Year Exporter Certanium 707 Welding Rod - Welding powder: E6013 – Tianqiao, The product will supply to all over the world, such as: Chile, Macedonia, Ireland, Our products are widely recognized and trusted by users and can meet continuously developing economic and social needs. We welcome new and old customers from all walks of life to contact us for future business relationships and achieving mutual success!

  • We are a small company that has just started, but we get the company leader's attention and gave us a lot of help. Hope we can make progress together!
    5 Stars By Althea from Italy - 2018.09.23 18:44
    The company comply with the contract strict, a very reputable manufacturers, worthy a long-term cooperation.
    5 Stars By Eve from Hamburg - 2018.05.22 12:13

    Send your message to us:

    Write your message here and send it to us

    Related Products